Polymer Property : Gardner Impact = 15.4 J
Polymer Property :
Gardner Impact =
15.4 J
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Gardner Impact
15.4
J
11.4
ft-lb
ASTM D5420-93
Multibase Multi-Pro® 4810 C White 47.7% Filler Content Polypropylene
Moisture content is 0.04%. Data provided by Multibase.