Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Gardner Impact = 15.3 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 20.8 J

@Thickness 3.18 mm,
Temperature -23.0 °C
15.3 ft-lb

@Thickness 0.125 in,
Temperature -9.40 °F
ASTM D3029
PolyOne Maxxam™ PPC-20C Nat Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Gardner Impact 20.8 - 20.8 J

@Temperature -23.0 - -23.0 °C
15.3 - 15.3 ft-lb

@Temperature -9.40 - -9.40 °F
Average value: 14.7 J Grade Count:1
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Gardner Impact 20.8 - 20.8 J

@Thickness 3.18 - 3.18 mm
15.3 - 15.3 ft-lb

@Thickness 0.125 - 0.125 in
Average value: 14.7 J Grade Count:1
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Gardner Impact 20.8 J

@Temperature 23.0 °C
15.3 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 63 mil
Axiall SP-7107 Rigid PVC, Molding
Georgia Gulf SP-7107 is a general purpose, electrical grade rigid vinyl injection molding compound characterized by excellent flow, heat stability, color hold and surface appearance. This makes it ..