Mechanical Properties Metric English Comments
Gardner Impact 11.7 J
8.60 ft-lb
ASTM D4228
CPC - Vycom CELTEC MARINE™ Expanded Foam PVC Polyvinyl Chloride
Celtec Marine is made from rigid expanded foam polyvinyl chloride (PVC) material whose combination of features makes it ideal for wood trim and plywood replacement in boat manufacturing. Its closed ..