Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 14.5 J | 10.7 ft-lb | ASTM D3029 |
Washington Penn PPH5CF5 Polypropylene, 50% Calcium Carbonate Filled UV Stabilized; Injection molding grade.Applications: Commonly used as a concentrate. High flow for thin wall parts requiring long-flow. Toys, small appliances, outdoor furniture.Data provided by W.. |