Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 10.2 J | 7.52 ft-lb | ASTM D5420-93 |
Multibase Multi-Pro® 3011 CHI Grey 29% Filler Content Polypropylene Data provided by Multibase. |
|||
Gardner Impact | 10.2 J | 7.52 ft-lb | ASTM D5420 |
PolyOne OnForce™ LFT LF5200-5001 EM Natural Polyolefin, Unspecified PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Gardner Impact | 10.2 J | 7.52 ft-lb | ASTM D5420 |
PolyOne OnForce™ LFT PP-30LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Gardner Impact | 10.2 J | 7.50 ft-lb | ASTM D5420 |
RheTech Products T10P250-00 10% Talc Reinforced Polypropylene Copolymer, Natural Applications: Fan shroudsCenter consolesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 10.2 J | 7.50 ft-lb | ASTM D5420 |
RheTech Products T10P250-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black Applications: Wire troughFan shroudsElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 10.2 J | 7.50 ft-lb | ASTM D5420 |
RheTech Products T12P600-01BG 12% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: Flipper panelClose out panelSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 10.2 J | 7.50 ft-lb | ASTM D5420 |
RheTech Products T12P600-430UVBG 12% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Interior 848 Black, Blow Molding Grade Applications: Flipper panelsSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 10.2 J | 7.52 ft-lb | ASTM D5420-93 |
Multibase Multi-Pro® 3019 CXUW High Gloss 30% TiO2 Filler Content Polypropylene Multi-Pro 3019 CXUW is a mineral reinforced polypropylene compound exhibiting high stiffness and impact characteristics. This material was specially formulated with UV stabilization for outdoor app.. |
|||
Gardner Impact | 10.2 J | 7.50 ft-lb | ASTM D5420 |
RheTech Products HP511-00 27% Talc Reinforced Polypropylene Copolymer, High Performance, Non-UV Stabilized, Natural Applications: Interior trimCenter consolesI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | >= 10.2 J | >= 7.50 ft-lb | |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Gardner Impact | 10.2 J | 7.50 ft-lb | ASTM D3029 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Gardner Impact | >= 10.2 J | >= 7.50 ft-lb | |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Gardner Impact | 10.2 J | 7.50 ft-lb | ASTM D3029 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Gardner Impact | >= 10.2 J | >= 7.50 ft-lb | |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Gardner Impact | 10.2 J | 7.50 ft-lb | ASTM D3029 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Gardner Impact | >= 10.2 J | >= 7.50 ft-lb | |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Gardner Impact | >= 10.2 J | >= 7.50 ft-lb | |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Gardner Impact | 10.2 J | 7.50 ft-lb | ASTM D3029 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Gardner Impact | >= 10.2 J | >= 7.50 ft-lb | |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Gardner Impact | 10.2 J | 7.50 ft-lb | ASTM D3029 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Gardner Impact | 10.2 J | 7.50 ft-lb | ASTM D3029 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Gardner Impact | 10.2 J | 7.52 ft-lb | ASTM D3029 |
Buckeye Polymers BP RPP 0511C Polypropylene, 5% Mineral Filled Increased flex w/ living hinge propertiesCalcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be cus.. |