Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792-91
Melt Flow 11 g/10 min
11 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 15.2 MPa
2200 psi
ASTM D638-95
Elongation at Break >= 500 %
>= 500 %
ASTM D638-95
Flexural Strength 20.0 MPa
2900 psi
ASTM D790-95
Flexural Modulus 0.931 GPa
135 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched NB
NB
ASTM D-256-93a
Gardner Impact 10.2 J
7.52 ft-lb
ASTM D5420-93