Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 0.655 J | 0.483 ft-lb | ASTM D3029 |
Plastics Group Polifil® M-40 40% Mica-Reinforced Polypropylene Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in l.. |