Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 0.600 J | 0.443 ft-lb | ASTM D3029 |
Adell EA-16 Homopolymer Polypropylene, 30% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Gardner Impact | 0.600 J | 0.443 ft-lb | ASTM D3029 |
Adell EA-18 Homopolymer Polypropylene, 40% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Gardner Impact | 0.600 J | 0.443 ft-lb | ASTM D3029 |
Adell EL-18 Homopolymer Polypropylene, 40% Mineral Filled; Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Gardner Impact | 0.600 J | 0.443 ft-lb | ASTM D3029 |
Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled Data provided by Adell Plastics, Inc. |