Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact | 126 - 134 J | 92.9 - 98.8 ft-lb | Notch Status Unknown |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Izod Impact | 126 - 133 J | 92.9 - 98.1 ft-lb | Notch Status Unknown |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Izod Impact | 126 - 134 J | 92.9 - 98.8 ft-lb | Notch Status Unknown |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Izod Impact | 126 - 133 J | 92.9 - 98.1 ft-lb | Notch Status Unknown |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |