Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact = 126 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact 126 - 134 J
92.9 - 98.8 ft-lb
Notch Status Unknown
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Izod Impact 126 - 133 J
92.9 - 98.1 ft-lb
Notch Status Unknown
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C)
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Izod Impact 126 - 134 J
92.9 - 98.8 ft-lb
Notch Status Unknown
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Izod Impact 126 - 133 J
92.9 - 98.1 ft-lb
Notch Status Unknown
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C)
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Copyright © lookpolymers.com All Rights Reserved