Mechanical Properties Metric English Comments
Izod Impact 80.0 J
59.0 ft-lb
Notched; ASTM D256
Flint Hills PP 23R2A Random Copolymer Polypropylene
Random copolymer, radiation sterilization resistant, Drug Master File (DMF) listed, USP Class VI certified, and FDA compliantFeatures: High contact clarity, non-blushing, toughness, impact, chemical..