Flint Hills PP 23R2A Random Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills PP 23R2A Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Random copolymer, radiation sterilization resistant, Drug Master File (DMF) listed, USP Class VI certified, and FDA compliantFeatures: High contact clarity, non-blushing, toughness, impact, chemical, solvent, stress crack resistance, stiffness, hardness, heat resistance, exceptional high clarity and impact strength.Applications: Blow molded: radiation sterilizable vials and bottles.FDA Notes: 21 CFR 177.1520 (c)3.2; under conditions of use B through H described in 21 CFR 176.170 Table 2Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Break >= 700 %
>= 700 %
ASTM D638
Modulus of Elasticity 1.015 GPa
147.2 ksi
ASTM D638
Flexural Modulus 0.940 GPa
136 ksi
ASTM D790
Izod Impact 80.0 J
59.0 ft-lb
Notched; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648