Mechanical Properties Metric English Comments
Dart Drop Total Energy 200 J/cm
0.375 ft-lb/mil
rotomolded sample; ISO 6603/2
Polimeri Europa Clearflex® RP 50 U Linear Medium Density Polyethylene
Clearflex RP 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RP 50 U show good mecha..
Dart Drop Total Energy 200 - 210 J/cm
0.375 - 0.393 ft-lb/mil
Average value: 208 J/cm Grade Count:13
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu..
Dart Drop Total Energy 200 - 220 J/cm
0.375 - 0.412 ft-lb/mil
Average value: 208 J/cm Grade Count:4
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i..
Dart Drop Total Energy 200 J/cm
0.375 ft-lb/mil
rotomolded sample; ISO 6603/2
Polimeri Europa Clearflex® RL 50 U Linear Medium Density Polyethylene
Clearflex RL 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha..