Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 210 J/cm | 0.393 ft-lb/mil | rotomolded sample; ISO 6603/2 |
Polimeri Europa Clearflex® RN 50 U Linear Medium Density Polyethylene Clearflex RN 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha.. |