Polymer Property : 200% Modulus = 1.86 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
200% Modulus 0.0128 GPa
1.86 ksi
ASTM D412
Dow Tyrin® CM2348P Formulation
FormulationTyrin® CPE Elastomer