Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.000660 GPa | 0.0957 ksi | ASTM D3574E |
Mearthane Durethaneâ„¢ M DM-715A Foam Polyurethane MDI backbone: ether.Shore 00 Hardness: 60Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |