Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.0133 GPa | 1.93 ksi | ASTM D412 |
UBE UBEPOL VCR617 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |