Polymer Property : 200% Modulus = 0.00586 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
200% Modulus 0.00586 GPa
0.850 ksi
ASTM D412
Lubrizol Estane® AG 4350 Thermoplastic Polyurethane
Type: Estane® AG 4350 is a polyether based aliphatic polyurethane specifically formulated to be used as an adhesive interlayer without the need for a glass surface primer. This polymer is designed..
200% Modulus 0.00586 GPa
0.850 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
200% Modulus 0.00586 GPa
0.850 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..