Mechanical Properties Metric English Comments
200% Modulus 0.00150 GPa
0.218 ksi
press cure 11 min./160ºC
TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications
Millathane 26 is a polyether polyurethane rubber compliant with the United States Code of Federal Regulations*, Title 21 parts 177.1680 and 177.2600. This polyurethane rubber is designed for food co..
200% Modulus 0.00150 GPa
0.218 ksi
press cure 11 min./160ºC
TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications
Millathane 26 is a polyether polyurethane rubber compliant with the United States Code of Federal Regulations*, Title 21 parts 177.1680 and 177.2600. This polyurethane rubber is designed for food co..