Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications

Category Polymer , Thermoset , Polyurethane, TS
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane 26 is a polyether polyurethane rubber compliant with the United States Code of Federal Regulations*, Title 21 parts 177.1680 and 177.2600. This polyurethane rubber is designed for food contact applications such as belting, rollers, seals, gaskets, linings, socks, boots, lagging, curtains, and hoses. Millathane 26 is peroxide-curable only.Typical Compound PropertiesMillathane 76 100.0Stearic Acid 0.3Ultrasil VN325TP-95 (DBEEA)2.0Struktol WB2221.0DiCup 40C4.0All information provided by TSE Industries
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
Mooney Viscosity 30 - 60

@Temperature 100 °C
30 - 60

@Temperature 212 °F
ML(1+4)
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
press cure 11 min./160ºC
Tensile Strength, Yield 23.4 MPa
3390 psi
press cure 11 min./160ºC
Elongation at Break 700 %
700 %
press cure 11 min./160ºC
100% Modulus 0.00110 GPa
0.160 ksi
press cure 11 min./160ºC
200% Modulus 0.00150 GPa
0.218 ksi
press cure 11 min./160ºC
300% Modulus 0.00230 GPa
0.334 ksi
press cure 11 min./160ºC
Tear Strength 29.1 kN/m
166 pli
Die C, press cure 11 min./160ºC
Descriptive Properties Value Comments
Appearance Pale to yellow sheets or bales
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved