Polymer Property : Izod Impact Resistance = 3.81 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Resistance >= 0.800 J/cm²
>= 3.81 ft-lb/in²
swinging hammer 0,1 DIN 51222; DIN 53453
Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated
Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH
Izod Impact Resistance >= 0.800 J/cm²
>= 3.81 ft-lb/in²
swinging hammer 0,1 DIN 51222; DIN 53453
Schwartz Technical Plastics LAMINEX® 2141 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled
Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH