Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | >= 0.800 J/cm² | >= 3.81 ft-lb/in² | swinging hammer 0,1 DIN 51222; DIN 53453 |
Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Izod Impact Resistance | >= 0.800 J/cm² | >= 3.81 ft-lb/in² | swinging hammer 0,1 DIN 51222; DIN 53453 |
Schwartz Technical Plastics LAMINEX® 2141 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |