Mechanical Properties Metric English Comments
Izod Impact Resistance 0.550 J/cm²
2.62 ft-lb/in²
ISO 180A
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-7-120BL is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance molding using..