Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 180A |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-7-120BL is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance molding using.. |