Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 0.350 J/cm² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Astryn BB73F Polypropylene Copolymer, Mineral Filled Key Features: high melt flow, high modulus, UV-stabilized, mineral-filled, high rigidity, good impact strength, good dimensional stability, good scratch and mar resistance, excellent processability,.. |