Material Notes:
Key Features: high melt flow, high modulus, UV-stabilized, mineral-filled, high rigidity, good impact strength, good dimensional stability, good scratch and mar resistance, excellent processability, low foggingApplications: door panels, map pockets bins, pillar moldings, seat belt guidesDescription: Astryn BB73F high melt flow, UV-stabilized, precolored mineral-filled polypropylene copolymer has a very good combination of rigidity, impact strength, dimensional stability, scratch and mar resistance and processability. It was designed for a variety of automotive interior trim applications.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792B
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ISO Method 2577
Melt Flow 19 g/10 min

@Load 2.16 kg,
Temperature 230 °C
19 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO Method R527
Elongation at Yield 4.0 %
4.0 %
ISO Method R527
Flexural Modulus 2.20 GPa
319 ksi
ISO Method 178
Izod Impact Resistance 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
30.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 114 °C
237 °F
ISO Method 180