Polymer Property : Puncture Energy = 3.10 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 4.20 J

@Load <=112 kg,
Temperature 23.0 °C
3.10 ft-lb

@Load <=247 lb,
Temperature 73.4 °F
Conditioned; ISO 6603-2
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers
PA 66, 30% glass fibers, injection molding, heat-ageing stabilized
Copyright © lookpolymers.com All Rights Reserved