Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 28.0 J @Thickness 2.50 mm, Temperature 23.0 °C |
20.7 ft-lb @Thickness 0.0984 in, Temperature 73.4 °F |
max load; ASTM D3763 |
Eastman Drystar 0601 Copolyester, Injection Molded This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Puncture Energy | 28.0 J @Thickness 2.50 mm, Temperature 23.0 °C |
20.7 ft-lb @Thickness 0.0984 in, Temperature 73.4 °F |
At Max load; ASTM D3763 |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |