Puncture Energy 2.60 J

@Load <=76.5 kg,
Temperature -30.0 °C
1.92 ft-lb

@Load <=169 lb,
Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modifiedInformation provided by LANXESS.