Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 2.60 J @Load <=76.5 kg, Temperature -30.0 °C |
1.92 ft-lb @Load <=169 lb, Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |