Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Puncture Energy = 2.21 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 3.00 J

@Load <=102 kg,
Temperature 23.0 °C
2.21 ft-lb

@Load <=225 lb,
Temperature 73.4 °F
ISO 6603-2
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant
PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS.
Puncture Energy 3.00 J

@Load <=85.7 kg,
Temperature 23.0 °C
2.21 ft-lb

@Load <=189 lb,
Temperature 73.4 °F
ISO 6603-2
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS.
Copyright © lookpolymers.com All Rights Reserved