Mechanical Properties Metric English Comments
Secant Modulus 0.689 GPa

@Strain 3.50 %,
Temperature 100 °C
99.9 ksi

@Strain 3.50 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi..
Secant Modulus 0.689 GPa

@Strain 3.60 %,
Temperature 100 °C
99.9 ksi

@Strain 3.60 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper..
Secant Modulus 0.689 GPa

@Strain 3.50 %,
Temperature 100 °C
99.9 ksi

@Strain 3.50 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%..
Secant Modulus 0.689 GPa

@Strain 3.60 %,
Temperature 100 °C
99.9 ksi

@Strain 3.60 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..