Polymer Property : Secant Modulus = 959 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 6.61 GPa

@Strain 1.48 %,
Temperature 40.0 °C
959 ksi

@Strain 1.48 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET)
20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol..