Polymer Property : Secant Modulus = 912.66 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 6.2925 GPa

@Strain 0.800 %,
Temperature 40.0 °C
912.66 ksi

@Strain 0.800 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti..