Polymer Property : Secant Modulus = 872 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 6.02 GPa

@Strain 1.53 %,
Temperature 40.0 °C
872 ksi

@Strain 1.53 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal..
Secant Modulus 6.01 GPa

@Strain 1.36981 %,
Temperature 40.0 °C
872 ksi

@Strain 1.36981 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..