Mechanical Properties Metric English Comments
Secant Modulus 5.67 GPa

@Strain 0.890 %,
Temperature 0.000 °C
823 ksi

@Strain 0.890 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Secant Modulus 5.67 GPa

@Strain 1.44 %,
Temperature -20.0 °C
823 ksi

@Strain 1.44 %,
Temperature -4.00 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66  (Unverified Data**)
30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa..
Secant Modulus 5.67 GPa

@Strain 0.980 %,
Temperature 40.0 °C
823 ksi

@Strain 0.980 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal..