Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.384 GPa @Strain 0.250 %, Temperature 40.0 °C |
55.7 ksi @Strain 0.250 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010 Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced.. |