Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.10 GPa @Strain 0.700 %, Temperature 0.000 °C |
450 ksi @Strain 0.700 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |