Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.46 GPa @Strain 3.70 %, Temperature 23.0 °C |
357 ksi @Strain 3.70 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |