Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.4175 GPa @Strain 3.20 %, Temperature -40.0 °C |
350.63 ksi @Strain 3.20 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |