Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.234 GPa @Strain 17.0 %, Temperature 23.0 °C |
34.0 ksi @Strain 17.0 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |