Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.09 GPa @Strain 2.60 %, Temperature 23.0 °C |
303 ksi @Strain 2.60 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Secant Modulus | 2.09 GPa @Strain 2.12 %, Temperature 23.0 °C |
303 ksi @Strain 2.12 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |