Polymer Property : Secant Modulus = 3.72 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 3.72 GPa

@Strain 0.730 %,
Temperature -20.0 °C
540 ksi

@Strain 0.730 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It..
Secant Modulus 3.72 GPa

@Strain 0.730 %,
Temperature -20.0 °C
540 ksi

@Strain 0.730 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati..
Secant Modulus 3.72 GPa

@Strain 2.40 %,
Temperature 80.0 °C
539 ksi

@Strain 2.40 %,
Temperature 176 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
Secant Modulus 3.72 GPa

@Strain 3.17 %,
Temperature 40.0 °C
539 ksi

@Strain 3.17 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf..