Mechanical Properties Metric English Comments
Secant Modulus 3.44 GPa

@Strain 1.54 %,
Temperature 40.0 °C
498 ksi

@Strain 1.54 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Secant Modulus 3.44 GPa

@Strain 0.800 %,
Temperature 100 °C
498 ksi

@Strain 0.800 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G15HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR NC010 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i..
Secant Modulus 3.44 GPa

@Strain 0.500 %,
Temperature 23.0 °C
499 ksi

@Strain 0.500 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
Secant Modulus 3.44 GPa

@Strain 0.430 %,
Temperature 23.0 °C
499 ksi

@Strain 0.430 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info..
Copyright © lookpolymers.com All Rights Reserved