Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.65 GPa @Strain 6.71 %, Temperature 40.0 °C |
240 ksi @Strain 6.71 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610
(Unverified Data**) 20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers |
|||
Secant Modulus | 1.65 GPa @Strain 2.96 %, Temperature 100 °C |
240 ksi @Strain 2.96 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610
(Unverified Data**) 20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers |
|||
Secant Modulus | 1.66 GPa @Strain 3.84 %, Temperature 40.0 °C |
240 ksi @Strain 3.84 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |