Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 235 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 1.62 - 10.2 GPa

@Temperature -40.0 - 100 °C
235 - 1480 ksi

@Temperature -40.0 - 212 °F
Average value: 5.73 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Secant Modulus 1.62 - 10.2 GPa

@Strain 0.250 - 3.50 %
235 - 1480 ksi

@Strain 0.250 - 3.50 %
Average value: 5.73 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Secant Modulus 1.62 GPa

@Strain 3.50 %,
Temperature 100 °C
235 ksi

@Strain 3.50 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
Secant Modulus 1.62 GPa

@Temperature 200 °C
235 ksi

@Temperature 392 °F
ASTM D882
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film
120 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 2.5 µm (0.1 mil) coating of Teflon® FEP on both sides.Kapton® Type HN film coated with Teflon® FEP fluoropolyme..
Secant Modulus 1.62 GPa

@Strain 0.620 %,
Temperature 23.0 °C
235 ksi

@Strain 0.620 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide..