Mechanical Properties Metric English Comments
Secant Modulus 1.62 - 10.2 GPa

@Temperature -40.0 - 100 °C
235 - 1480 ksi

@Temperature -40.0 - 212 °F
Average value: 5.73 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Secant Modulus 1.62 - 10.2 GPa

@Strain 0.250 - 3.50 %
235 - 1480 ksi

@Strain 0.250 - 3.50 %
Average value: 5.73 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..