Mechanical Properties Metric English Comments
Secant Modulus 1.52 GPa

@Strain 0.190 %,
Temperature 40.0 °C
220 ksi

@Strain 0.190 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi..
Secant Modulus 1.52 GPa

@Strain 0.190 %,
Temperature 40.0 °C
220 ksi

@Strain 0.190 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT)
Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided..
Secant Modulus 1.52 GPa

@Strain 6.00 %,
Temperature -40.0 °C
220 ksi

@Strain 6.00 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 300CP BK642 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc..
Secant Modulus 1.52 GPa

@Strain 0.500 %,
Temperature 80.0 °C
220 ksi

@Strain 0.500 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring ..
Secant Modulus 1.52 GPa

@Strain 0.500 %,
Temperature 80.0 °C
220 ksi

@Strain 0.500 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear ..