Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.5125 GPa @Strain 4.00 %, Temperature 80.0 °C |
219.37 ksi @Strain 4.00 %, Temperature 176 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |