Polymer Property : Secant Modulus = 2.47 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 2.47 GPa

@Strain 2.29 %,
Temperature 0.000 °C
358 ksi

@Strain 2.29 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It..
Secant Modulus 2.47 GPa

@Strain 2.29 %,
Temperature 0.000 °C
358 ksi

@Strain 2.29 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati..
Secant Modulus 2.47 GPa

@Strain 0.700 %,
Temperature 100 °C
359 ksi

@Strain 0.700 %,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa..